Compare commits
2 Commits
fe8a7209b3
...
f875f32177
Author | SHA1 | Date | |
---|---|---|---|
f875f32177 | |||
506984b69c |
13
uni/mmme/1028_statics_and_dynamics/dynamics.md
Executable file
13
uni/mmme/1028_statics_and_dynamics/dynamics.md
Executable file
@ -0,0 +1,13 @@
|
||||
---
|
||||
author: Akbar Rahman
|
||||
date: \today
|
||||
title: MMME1028 // Dynamics
|
||||
tags: [ uni, mmme1028, dynamics ]
|
||||
uuid: e6d3a307-b2e6-40e3-83bb-ef73512d69ad
|
||||
---
|
||||
|
||||
# Circular Motion
|
||||
|
||||
$$a_c = r\omega^2$$
|
||||
|
||||
$$a = r\alpha \hat{e}_\theta - r\omega^2\hat{e}_r$$
|
Binary file not shown.
After Width: | Height: | Size: 2.4 KiB |
Binary file not shown.
After Width: | Height: | Size: 2.5 MiB |
Binary file not shown.
After Width: | Height: | Size: 418 KiB |
Binary file not shown.
After Width: | Height: | Size: 142 KiB |
Binary file not shown.
After Width: | Height: | Size: 63 KiB |
@ -1090,7 +1090,7 @@ As you decrease grain size, you get more grain boundaries which basically create
|
||||
to prevent slip.
|
||||
|
||||
This is because a dislocation would have to change orientation across a grain boundary and "ionic
|
||||
disorder in the grain boundary results in discontinuity of slip" (A.B Seddon University of
|
||||
disorder in the grain boundary results in discontinuity of slip" (A.B Seddon, University of
|
||||
Nottingham 2020) (I think that's repeating it but it said it on the slideshow sooo...).
|
||||
|
||||
So for any given metal, the fine grained is harder and has greater yield stress than the coarse
|
||||
@ -1104,6 +1104,41 @@ where $d$ is the grain size and $\sigma_0$ and $k_y$ are material constants.
|
||||
|
||||
Therefore a plot of $\sigma_{yield}$ against $d^{-0.5}$ would results in a straight line.
|
||||
|
||||
## Heat Treatment of Metals
|
||||
|
||||
These processes are to change a material's mechanical properties, not change its shape.
|
||||
|
||||
### Phase Diagrams
|
||||
|
||||
Here is an example of a *two component phase diagram* with a familiar system:
|
||||
|
||||
![](./images/vimscrot-2022-03-07T14:16:57,570858805+00:00.png)
|
||||
|
||||
The component in this case are sugar and water, but not syrup.
|
||||
|
||||
A *phase* is a chemically and physically distinct species as we can have a change in phase that goes
|
||||
from solid to solid.
|
||||
|
||||
The *solubility limit* is the maximum concentration for which only a solution occurs.
|
||||
In the case of this system, thee limit increases with temperature.
|
||||
|
||||
Here is a generic phase diagram for a generic *A-B* system:
|
||||
|
||||
![](./images/vimscrot-2022-03-07T14:26:08,092894184+00:00.png)
|
||||
|
||||
- L - liquid
|
||||
- $\alpha$ --- a solid phase but still a solution. B can dissolve into A
|
||||
- $\beta$ --- a solid phase but still a solution. A can dissolve into B
|
||||
|
||||
### Annealing
|
||||
|
||||
Annealing is a process by which a component is heated to remove the effects of cold work.
|
||||
|
||||
![](./images/vimscrot-2022-03-07T14:15:01,296649522+00:00.png)
|
||||
|
||||
These are diffusional processes and only occur at high temperatures.
|
||||
The driver for diffusion is the removal of high energy defects from the system.
|
||||
|
||||
# Diffusion
|
||||
|
||||
Diffusion is atomic or ionic movement down a concentration gradient.
|
||||
|